New superalloy could cut carbon emissions from power plants

Alert
Current COVID-19 Community Level: LOW (March 17) CDC COVID-19 County Check

Sandia scientists, collaborating with researchers at Ames National Laboratory, Iowa State University and Bruker Corp., used a 3D printer to create a high-performance metal alloy, or superalloy, with an unusual composition that makes it stronger and lighter than state-of-the-art materials currently used in gas turbine machinery. The findings could have broad impacts across the energy sector as well as the aerospace and automotive industries, and hints at a new class of similar alloys waiting to be discovered. The team published their findings in the journal Applied Materials Today

News Link: New superalloy could cut carbon emissions from power plants